Structural concrete elements deployed across coastal zones, marine installations, and regions reliant on de-icing salts encounter severe degradation driven by the simultaneous intrusion of corrosive chemicals and sustained service loads. A team of civil engine

Illustrative imageIllustrative image

Structural concrete elements deployed across coastal zones, marine installations, and regions reliant on de-icing salts encounter severe degradation driven by the simultaneous intrusion of corrosive chemicals and sustained service loads. A team of civil engineers led by Kaiqi Wang and Tan Wang evaluated thirty-nine concrete beams to investigate how combining glass fiber-reinforced polymer bars with conventional steel rebars protects against this destructive synergy. Their experimental findings reveal that hybrid-reinforced beams retain substantially higher ultimate flexural capacity than either purely steel-reinforced or purely polymer-reinforced members when subjected to coupled wetting-drying cycles in composite magnesium sulfate and sodium chloride solutions under continuous mechanical stress. While conventional steel-reinforced beams suffered ultimate load reductions between 18.7 and 35.2 percent, and fully polymer-reinforced beams experienced capacity losses between 23.5 and 42.3 percent, the hybrid beams limited flexural degradation to between 11.6 and 27.6 percent across equivalent exposure regimes, demonstrating enhanced resilience against aggressive environmental deterioration.

Reinforced concrete structures in aggressive marine and saline soil environments face continuous chemical attack from chloride and sulfate ions that penetrate through porous cement paste. Chloride ions trigger active electrochemical corrosion of conventional steel reinforcement, inducing rust expansion, cover cracking, and loss of reinforcement cross-sectional area, while sulfate ions react with hydration products to form expansive crystals that generate destructive internal pressures. In recent years, glass fiber-reinforced polymer rebars have emerged as a non-corrosive alternative because of their high tensile strength and immunity to electrochemical oxidation. However, polymer bars exhibit a comparatively low elastic modulus of approximately 53 gigapascals, compared to 200 gigapascals for structural steel. This flexibility leads to rapid stiffness degradation, wider cracks, and extensive midspan deflections once surrounding concrete cracks under service loads, restricting the practical deployment of purely polymer-reinforced elements in flexural structural applications requiring strict serviceability and deformation control.

To reconcile the competing demands of chemical durability and structural stiffness, the researchers implemented a hybrid reinforcement strategy that strategically locates corrosion-resistant glass fiber-reinforced polymer bars at vulnerable outer corner positions while retaining a central longitudinal steel rebar within the main tensile zone. The experimental campaign evaluated three distinct beam configurations cast with C30 concrete having a twenty-eight-day cube compressive strength of 35.4 megapascals: Group A contained conventional HRB400 steel rebars, Group B incorporated pure glass fiber-reinforced polymer bars, and Group C utilized the hybrid arrangement with two corner polymer bars flanking a central steel rebar.

The experimental matrix comprised thirty-nine beam specimens with rectangular cross-sections measuring 100 millimeters in width, 150 millimeters in depth, and 1100 millimeters in overall length, reinforced longitudinally to achieve a reinforcement ratio of 1.83 percent alongside transverse steel stirrups spaced at 35 millimeters in the shear span and 70 millimeters elsewhere. To accelerate environmental degradation and simulate vulnerable infrastructure elements, the team specified a compact concrete cover thickness of only 10 millimeters, deliberately shortening the diffusion distance for aggressive chemical species and expediting cover cracking. The beams were categorized across combinations of cyclic exposure durations, encompassing unexposed control states alongside 90 and 180 wetting-drying cycles, conducted either under ambient laboratory temperatures or within an accelerated thermal regime maintained at 45 degrees Celsius. Sustained flexural loading was maintained at thirty percent of each configuration’s unexposed ultimate bearing capacity, applied via mechanically locked spring rigs to induce initial surface cracks exceeding 0.2 millimeters before immersion.

Environmental simulation subjected the specimens to alternating cycles consisting of eight hours of total immersion in a composite salt solution containing 20 grams per liter of sodium chloride and 50 grams per liter of magnesium sulfate, followed by sixteen hours of forced drying at a controlled wetting-to-drying ratio of one to two. Material testing on accompanying concrete cubes revealed a complex staged degradation mechanism governed by chemical kinetics. During initial cycles up to 90 iterations, compressive strength exhibited slight temporary increases attributable to continued matrix hydration and the physical deposition of sulfate reaction products within capillary pores, which temporarily densified the cementitious micro-structure. However, by 180 cycles, progressive crystallization pressures from accumulating expansive products coupled with repeated moisture gradients initiated micro-cracking networks, causing marked compressive strength reductions that mirrored the observed structural decline in beam load-carrying capacity and sectional integrity.

Concurrent material tests conducted on the reinforcing rebars detailed distinct deterioration pathways that directly governed structural responses during subsequent four-point bending tests. The HRB400 steel bars experienced continuous electrochemical corrosion under chloride attack, resulting in progressive decreases in both effective tensile yield strength and residual cross-sectional area, though surface accumulations of corrosion products moderately slowed ion transport rates during later cycles. Conversely, while the glass fiber-reinforced polymer bars avoided electrochemical pitting, exposure to elevated temperatures and moisture diffusion through the protective resin matrix caused localized matrix plasticization and hydrolysis along the fiber-matrix interfaces. Despite these environmental impacts, the tensile modulus of the polymer bars remained essentially stable, ensuring that the hybrid-reinforced specimens maintained reliable tensile capacity across prolonged exposure intervals, even as the central steel rebar underwent gradual cross-sectional loss.

When subjected to post-exposure four-point bending after complete mechanical unloading, all beam specimens exhibited a multi-stage load-deflection response comprising an initial elastic phase, a post-cracking stage with reduced bending stiffness, and a final nonlinear ascent toward ultimate capacity. For specimens that had undergone coupled exposure with sustained loading, this behavioral transition appeared significantly smoother because pre-existing mechanical cracks had already degraded the gross sectional moment of inertia before the final testing phase began. The initial flexural stiffness of reference control beams was measured at 39.15 kilonewtons per millimeter for Group A, 28.04 for Group B, and 30.91 for Group C. The coupled interaction of sustained mechanical stress and 45-degree composite-salt cycling caused severe stiffness losses, decreasing the initial stiffness of hybrid beams by 37.4 percent after 90 cycles and 6.4 percent after 180 cycles relative to unloaded counterparts.

Structural failure modes shifted noticeably under the influence of severe environmental damage, moving from standard flexural failure dominated by concrete compressive crushing toward sudden shear-compression failures within the shear span. In uncorroded benchmark testing, unexposed hybrid beam C-0 sustained an ultimate flexural load of 118.0 kilonewtons, failing through compressive crushing of the uppermost concrete fibers. After undergoing 180 coupled cycles at 45 degrees Celsius under continuous thirty percent sustained loading, the average ultimate capacity of hybrid specimens C-8 decreased to 85.85 kilonewtons, and both duplicate beams experienced shear-compression failure. The researchers observed that the combination of diagonal crack propagation, corrosion-induced bond slip, and localized concrete softening undermined the shear transfer mechanisms across the shear span, demonstrating that prolonged coupled exposure threatens not only normal-section flexural equilibrium but also member-level transverse shear resistance.

Reinforcement strain measurements gathered across the midspan sections confirmed that hybrid beams developed pronounced internal force redistribution between the differing reinforcement materials during monotonic loading. At moderate load levels prior to rebar yielding, the higher elastic modulus of the retained central steel bar attracted greater tensile stress, effectively stiffening the cracked cross-section and restraining midspan crack dilation. Once the steel strain reached the nominal yield threshold of approximately 2300 microstrain, incremental tensile stresses shifted smoothly onto the intact outer glass fiber-reinforced polymer bars, enabling steady capacity growth without abrupt structural collapse.

To assist structural engineers in forecasting residual load capacities in harsh marine environments, the authors established a mechanical capacity prediction model grounded in sectional strain compatibility, internal force equilibrium, and empirical material degradation functions. The formulation incorporates time-dependent equations describing the decay of concrete compressive strength, the progressive reduction in steel yield strength and bar area, and the temperature-dependent retention of glass fiber polymer tensile capacity. When validated against the seven tested hybrid-reinforced concrete beams that failed through concrete compressive crushing, the theoretical framework yielded predicted-to-measured ultimate capacity ratios between 0.80 and 0.98, achieving a mean predictive ratio of 0.863 with a standard deviation of 0.066. Because all model predictions remained strictly below actual measured capacities, the authors concluded that the analytical formulation provides a reliable and conservative methodology for the structural safety assessment of hybrid-reinforced concrete beams in corrosive coastal infrastructure.

Subject of Research: Flexural degradation and durability of hybrid GFRP-steel reinforced concrete beams under combined environmental exposure and sustained structural loading

Article Title: Flexural degradation of GFRP-steel hybrid-reinforced concrete beams under coupled composite-salt wetting-drying exposure and sustained loading

Article References: Wang, K., Wang, T., Yuan, Z., Ye, X., & Yang, F. (2026). Flexural degradation of GFRP-steel hybrid-reinforced concrete beams under coupled composite-salt wetting-drying exposure and sustained loading. Case Studies in Construction Materials, 25, Article e06756. https://doi.org/10.1016/j.cscm.2026.e06756

Image Credits: AI Generated

DOI: 10.1016/j.cscm.2026.e06756

Keywords: structural engineering, reinforced concrete, GFRP bars, hybrid reinforcement, composite salt exposure, wetting-drying cycles, sustained loading, flexural degradation, concrete durability, chloride corrosion, sulfate attack, bearing capacity, shear-compression failure, strain compatibility, concrete crushing, energy dissipation, deformability factor

News Source: Denise Maddox. (November 25, 2026). Hybrid Steel and Polymer Concrete Beams Retain Superior Load Capacity Under Marine Salt. Scienmag.